真石漆空鼓脱落原因有以下几个方面

日期:2016年7月27日 浏览[874]

 

1) 作业人员技术水平低, 责任心不强,对薄弱环节未采取有效防范措施,如喷枪压力选择不当、口径偏大等。


1) operation personnel technical level is low, the responsibility is not strong, the weak link has not taken effective preventive measures, such as the pressure of the spray gun is improper, the caliber is too large.


2) 在阴阳角、管根边等处,基层墙面抹灰班组处理不到位、不平整、不顺直,真石漆施工班组也未做好交接检工作,未作进一步深化处理,留下隐患;注册食品公司


2) in the Yin and yang angle and Guan Genbian, team of grassroots plastering metope processing does not reach the designated position, not smooth, not smooth straight, lacquer construction team also did not do a good job handover inspection work, without further processing, leaving hidden dangers;


3) 在真石漆乳液配方方面,有些厂家为了降低成本,乳液用量偏少,辅剂用量偏多,导致粘结力下降;


3) in lacquer emulsion formulation, some manufacturers in order to reduce costs, less than normal amount of emulsion, auxiliary agent amount slants much, resulting in decrease of bond strength;

4) 腻子与墙体基层粘结力差,腻子成分掺假;


4) and the wall base bonding putty, putty adulteration;


我们考察过许多用真石漆施工外墙的项目,发现许多地方真石漆产生空鼓脱落。特别是在阴阳角处、窗台处、管根边、受雨水影响较大的墙面处等相对薄弱的部位, 真石漆空鼓脱落更为突出。


We visited many stone construction of exterior wall project, found that many places have Konggu off lacquer. Especially in the angle of yin and Yang, the window, Guan Genbian, rain affected relatively weak parts of the Great Wall at the other, the lacquer Konggu off is more prominent.

 

安徽真石漆官方网站:http://www.ahzbj.com/

 

最新内容:



上一篇: 真石漆施工时颜色发黄和遇水发花
下一篇: 克服外墙真石漆施工中的质量通病采取相应的措施

安徽新型涂料有限公司 合肥墙绘公司 合肥网络布线版权所有 Copyright  2010 All Right Reserve 免责声明 皖ICP备11002092号 合肥网站制作:合肥网络公司

安徽省合肥市双凤工业园 网址:http://www.ahzbj.com/  网站地图