真石漆的施工条件和产生色差大的原因

日期:2016年7月26日 浏览[884]

产生色差大的原因可能与以下因素有关:


The reason for the large color difference may be related to the following factors:


(1) 每项施工材料用量没有一次备足,不同批材料的颜色有偏差,而造成色差;


(1) the amount of each construction materials have an ample supply of different material color deviation caused by chromatic aberration;


(2) 施工作业人员的技术水平高低不一,造成喷涂厚度不均,局部偏薄而形成色差;


(2) the technical level of construction workers is different, resulting in uneven coating thickness, partial thin and the formation of color;


(3) 受天气影响,墙面淋雨后,由于赶工期,局部部位未能在干燥的作业环境下施工,造成色差;

(3) affected by the weather, the wall after being out in the rain, because of the duration, local site failed in dry working environment construction and cause color;


(4) 调色不均,造成色差。


(4) uneven color, color difference.


施工条件


Construction condition


(1) 墙面干燥, 含水率小于10%,pH小于10,施工气温大于5℃,相对湿度小于85%。


(1) the wall surface is dry, the moisture content is less than 10%, the pH is less than 10, the construction temperature is greater than 5, and the relative humidity is less than 85%.


(2) 墙面基层平整, 各抹灰层结合牢固,无浮灰、油污等附着物。


(2) the primary wall formation, the plaster layer firmly, no dust, grease and other attachments.


(3) 墙面上的各种临时洞口全部修补完毕,并符合施工要求。


(3) all kinds of temporary holes on the wall to complete the repair, and in line with the requirements of the construction.

 

安徽真石漆官方网站:http://www.ahzbj.com/ 

 

最新内容:



上一篇: 浅谈水性多彩涂料的施工工艺水泥粗糙面注意事项
下一篇: 真石漆施工时颜色发黄和遇水发花

安徽新型涂料有限公司 合肥墙绘公司 合肥网络布线版权所有 Copyright  2010 All Right Reserve 免责声明 皖ICP备11002092号 合肥网站制作:合肥网络公司

安徽省合肥市双凤工业园 网址:http://www.ahzbj.com/  网站地图