日期:2016年6月30日 浏览[1080]

 

 

1)控制适当的涂料粘度,以正确的方法喷涂适量漆液;


2)选择好板材,或先刷1-2遍底得宝(封闭漆)封闭木眼,刮腻子填补缝隙,并打磨平整;


3)保持良好的排气;


4)调好油漆后应尽快在4小时内施工完。

5)选用较细的砂纸认真仔细打磨好;


6)选用厂家提供的配套稀释剂,或添加挥发慢的溶剂;


7)要有良好的涂装作业温湿度,要适当加入防白水等慢干溶剂;


8)清理干净被涂物面;


9)待漆膜完全干燥后才可进行抛光,并选择蜡的细度;


1) to control the proper viscosity of the paint, in order to correct the method of spraying amount of paint;


2) choose a good plate, or first brush 1-2 times of base depot (closed paint) wood closed eyes, putty to fill the gap, and grind;


3) keep good exhaust;


4) the paint should be adjusted as soon as possible after the construction of 4 hours.


5) use a fine sandpaper carefully burnish;


6) selection of manufacturers to provide matching diluent, or add a volatile solvent;


7) to have a good coating temperature and humidity, to be appropriate to join the anti white water, such as slow dry solvent;


8) clean up the coated material surface;


9) after the film is completely dry before polishing, and select the fineness of the wax;

 

 

官方网站:http://www.ahzbj.com

最新内容:



上一篇: 浅谈涂膜成雾状不能获得预期的光泽的原因
下一篇: 浅谈涂料施工时出现咬底的原因是什么

安徽新型涂料有限公司 合肥墙绘公司 合肥网络布线版权所有 Copyright  2010 All Right Reserve 免责声明 皖ICP备11002092号 合肥网站制作:合肥网络公司

安徽省合肥市双凤工业园 网址:http://www.ahzbj.com/  网站地图